Magnetic Flow Conditioners - Do They Work?

Status
Not open for further replies.

Hookem

Mechanical
Jan 29, 2003
96
Linear Kinetic Devices, Magnetic Flow Conditioners, Rare Earth Magnets, etc. as put out by various manufacturers claim to align particles in flowing streams of water, gasoline, oil, etc., etc. and rid those streams of undesireable characteristics. But, are there any hard scientific, objective proving (or disproving) of these claims?
 
Replies continue below

Recommended for you



to the snake-bit and well informed, the short answer is no

 
So true. Consensus demonstrated, for example, by: