I have a question for MANDATORY APPENDIX 20 20-2.
What kind of two test specimens sampling for app 20-2 ?
(1) two test specimens for each plate.
(2) two test specimens for each tubesheet
(3) two test specimens for each heat number
Test specimens, in addition to those required by the
material specifications, shall be taken in a direction paral-
lel to the axis of the hub and as close to the hub as prac-
tical, as shown in Figure UW-13.3. At least two tensile test
specimens shall be taken from the plate in the proximity
of the hub with one specimen taken from the center third
of the plate width as rolled, and the second specimen ta-
ken at 90 deg around the circumference from the other
specimen. Both specimens shall meet the tensile and yield
requirements of the SA material specification. All dimen-
sional requirements of Figure UW-13.3 shall apply.
I have a question for MANDATORY APPENDIX 20 20-2.
What kind of two test specimens sampling for app 20-2 ?
(1) two test specimens for each plate.
(2) two test specimens for each tubesheet
(3) two test specimens for each heat number
Test specimens, in addition to those required by the
material specifications, shall be taken in a direction paral-
lel to the axis of the hub and as close to the hub as prac-
tical, as shown in Figure UW-13.3. At least two tensile test
specimens shall be taken from the plate in the proximity
of the hub with one specimen taken from the center third
of the plate width as rolled, and the second specimen ta-
ken at 90 deg around the circumference from the other
specimen. Both specimens shall meet the tensile and yield
requirements of the SA material specification. All dimen-
sional requirements of Figure UW-13.3 shall apply.