Can someone give me details on how and what are the manufactureing process of making magnets(neodymium). thanks!
 
Replies continue below

Recommended for you

Did you try Google?

Stick this phrase in there: how neodymium magnets are made

Here are the first four hits, since I was curious and I felt like looking it up myself:





Best to you,

Goober Dave

Haven't see the forum policies? Do so now: Forum Policies
 
Following Steps are for sintered NdFeB Magnet
1. Raw Material mixing
2. Strip Casting
3. Hydrogen Decrepitation
4. Jet Milling
5. Pressing
6. Sintering
7. Annealing
8. Machining
9. Coating
10. Magnetizing
11. Inspection
12. Packing
13. Forwarding