I am presently looking for a method of applying a ring markerband on a wire that has been coated with a .0003" layer of PTFE. The PTFE used is dark green, and I need something that will adhere to the PTFE as well as giving a good color contrast. Minimal amount of increase in overall wire thickness is important.

Does any one have an idea.
 
Replies continue below

Recommended for you

Have you considered laser marking? There are a lot of laser marker suppliers out there - Control Micro Systems, Telesis, TDK to name a few.
 
We have tried laser, but the mark is dark grey, not very good contrast to our dark green coat.
 