Anyone know a reference to masonry allowable stress values/formulas for an unreinforced masonry arch (I have the f'm values for the brick and mortar from the ASTMs)? The allowable values given by ACI 530 Section 2.2 do not seem to apply for an arch (h/r ratio refers to the height of a column or wall).

Any help is greatly appreciated.
 
Replies continue below

Recommended for you

You might want to look for a program called Ring for analysing masonry arches

Dik
 
Technical Notes on Brick Construction #31A
"Structural Design of Brick Masonry Arches"
Table 1, p4
 