I would like to know the Yield Strenght and the Tensile Streght of a French Material called A-48C.3S, which chemical composition is:

C S P S+P Si Mn
A-48C.3S 0,22 0,04 0,04 0,07 0,35 0,6



Best Regards
Ivan



Ivan
KFC -Thermall & Mechanical Consulting
 
Replies continue below

Recommended for you

The heat treatment was stress relief.