I'm in the process of building a heavily modified, somewhat experimental, motorcycle. (two stroke)
I have the machining know how but am a bit confused by the material choices open to me.
I need to know what would be the best type of billet aluminium for the following applications & what heat treatments, etc, if any, these would require;
1) top & bottom fork yokes & fork bottoms / caliper mounts.
2) brake calipers (would the bores need special treatment?)
3) crank cases
4) barrels (I intend to have these nicasil plated)
I have looked into it & noted the materials a few aftermarket companies are using but don't know if these are best or how they have been treated.
Hope you guys can help.
Thanks.
I'm in the process of building a heavily modified, somewhat experimental, motorcycle. (two stroke)
I have the machining know how but am a bit confused by the material choices open to me.
I need to know what would be the best type of billet aluminium for the following applications & what heat treatments, etc, if any, these would require;
1) top & bottom fork yokes & fork bottoms / caliper mounts.
2) brake calipers (would the bores need special treatment?)
3) crank cases
4) barrels (I intend to have these nicasil plated)