Hi , We are trying to get the Manway flange face of our 50T pressure vessel machined and to make sure we will be within/above, the minimum thickness after machining we want to initially carry out a calculation to determine the minimum thickness. The problem is the design data on the drawing of the pressure vessel says its a BS1501-151-grade C material spec. The service provider does not have any record of this spec and I cant seem to see any info on the net.

Can someone help? Could the info on the drawing be wrong and there is no BS1501-151-grade C? Is this spec known by any other spec? is there an equivalent if this does not exist anymore?

Charles
 
Replies continue below

Recommended for you

PD 5500 only mentions Type A and B.
Type A and B are identical alloys.
Type A guarantees properties at ambient temperature.
Type B is the same as Type A with additional guarantee of elevated temperature properties.

I can't think what type C would be for. Low Temperature?
 