Aug 8, 2017 #1 ZHIYAR Mechanical Aug 8, 2017 3 0 0 IQ Dears Can I use fitting material A420 WPL6 instead of A234WPB. Regards
Aug 8, 2017 #2 XL83NL Mechanical Mar 3, 2011 3,043 0 36 NL That depends on a number of factors, like the application, service conditions, design code, engineering secifications, etc.. Without such information questions like these are impossible to answer. Upvote 0 Downvote
That depends on a number of factors, like the application, service conditions, design code, engineering secifications, etc.. Without such information questions like these are impossible to answer.
Aug 8, 2017 #3 david339933 Industrial Jun 15, 2011 1,204 0 0 CA Keeping in mind what XL83NL stated, often yes. SA420 WPL6 is often used in lieu of SA-234 WPB when impacts are required. Upvote 0 Downvote