200
We are looking for alternate material for an application where a glass filled PEI (ultem) is currently used. There are a few high precision features in the finished part so I am looking for a material that has good dimensional stable during and after machining (.0005 hole tolerances). Other important characteristics would be low water absorption, compatible epoxies for bonding, operating temps of 85+ C, and chemical resistance to common household cleaning solvents (such a wide range that I hesitate to list them all). The material cannot be electrically conductive.

Peek is being explored but I'd appreciate any suggestions.

thanks
 
Replies continue below

Recommended for you

PPO (Noryl) might be an option. PPSU or some of its sisters are another possibility, but I've never machined it.
 