i need advise for materrial selection for h2s removal pressure vessel for gas
this pressure vessel will be used for h2s removal which the inlet gas contain sulfur 150 ppm
the pressure inlet is 15 psig, and the gas temeprature 125 deg.F
ijust thinking to use carnon steel with suitable material for cladding
please advise which material should be used for pressure vessel
pressure diameter is 3.2 meters, and tangent to tangent length is 6 meters