Materials
Jan 20, 2007
250
what is the maximum content of nickel in the H13 steels ?
All the CODES AISI, German, french and others don't say any thing about the nickel on the H13 steel.

Thanks in advance

 
Replies continue below

Recommended for you

Normally when Ni is not a direct alloying element,the maxium permissible limits is 0.5%.

H13,grade steel does not have Ni as an alloying element it can be present as trace element only limited to 0.5% max.

I have not failed. I've just found 10,000 ways that won't work." — Thomas Edison
_____________________________________
 
ASTM A 681 Standard Specification for Tool Steels Alloy states:

nickel plus copper equal 0.75 % max
 