Apr 24, 2012 #1 Q1P Mechanical Dec 19, 2011 1 0 0 PH I am designing a stainless pressure vessel with -104C MDMT. But during in compress run, the required MDMT is only -48C. I'm trying to check the impact test,but the problem is still the same. What should I do?