Dec 3, 2004 #1 gerryk Materials Nov 12, 2003 3 0 0 GB Where can I get a free up to date metal corrosion table, suitable for reference in the valve industry.
Where can I get a free up to date metal corrosion table, suitable for reference in the valve industry.
Dec 3, 2004 #2 EdStainless Materials May 20, 2004 15,893 0 36 US Free, no. Very good, yes. Buy the Comapss Corrosion Guide. It is very complete and covers metals and non-metals. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm Upvote 0 Downvote
Free, no. Very good, yes. Buy the Comapss Corrosion Guide. It is very complete and covers metals and non-metals. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm
Dec 3, 2004 #3 metengr Materials Oct 2, 2003 15,478 0 0 US This web site may be of help. Review the attachment and down load the file. http://www.cranevalve.com/pdfs/aloyco/appdata.pdf Upvote 0 Downvote
This web site may be of help. Review the attachment and down load the file. http://www.cranevalve.com/pdfs/aloyco/appdata.pdf
Dec 9, 2004 #4 mshimko Materials Oct 27, 2004 364 0 0 US ASM also has a very good handbook; the title is "Handbook of Corrosion Data". Upvote 0 Downvote