Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

MIC in Carbon Steel receptacle filled with still deoxygenated water

Status
Not open for further replies.

upbubble

Marine/Ocean
Nov 3, 2005
1
I am looking at a carbon steel receptacle (holding tank)filled with deoxygenated water. I am concerned with MIC action. Are there any recommended biocides that should be added to the water?
Thank you,
Charley Harvilicz,
NACE CIP 206
SSPC Protective Coatings Specialist
 