Apr 11, 2014 #1 CREAAM Materials Mar 7, 2013 9 0 0 GB Can you get bacteria activity (MIC) in wet gas systems and if you have dry gas injection does that eliminate any microbial activity downstream.
Can you get bacteria activity (MIC) in wet gas systems and if you have dry gas injection does that eliminate any microbial activity downstream.
Apr 11, 2014 #2 brimmer Petroleum Mar 26, 2007 349 0 0 CA Yes, you can have MIC in wet gas systems, and often do. I have seen MIC in dry gas systems as well, but this is generally the exception rather than the norm. As alwaysm depends on conditions from drilling to processing. Upvote 0 Downvote
Yes, you can have MIC in wet gas systems, and often do. I have seen MIC in dry gas systems as well, but this is generally the exception rather than the norm. As alwaysm depends on conditions from drilling to processing.