Jul 10, 2009 #1 kkg123 Mechanical May 12, 2002 32 0 0 IN please let me know "mild steel (Indian)" equivalent gradein En. thank you kkg123
Jul 12, 2009 #2 MikeMet Chemical Dec 11, 2008 164 0 0 US Mild steel is generic term that could mean one of many grades of low carbon steel. Back in my old days it meant carbon steels with carbon content of 0.15 - 0.30%. I don't think a spec or equivalent can be applied without more information. Upvote 0 Downvote
Mild steel is generic term that could mean one of many grades of low carbon steel. Back in my old days it meant carbon steels with carbon content of 0.15 - 0.30%. I don't think a spec or equivalent can be applied without more information.