Mineral_Processing_Electroplating_Example

Status
Not open for further replies.

Redskinsdb21

Mining
May 4, 2009
45
If I want to know how much Gold is being electroplated onto Carbon during an electroplating example, how would I calculate this? Use Faradays law or other techniques?
 
Replies continue below

Recommended for you

1948 edition of Metals Handbook page 1107, "With 24-carat deposits, the weight laid down per ampere-hour may approach 7.3 g..."

This is not in reference to any particular substrate such as Carbon.

I don't know if this helps or not.