Jun 25, 2009 #1 gwelch123 Mechanical Oct 11, 2007 12 0 0 US What is the minimum API 1104 NDE requirements? RT, VT, PT etc..
Jun 25, 2009 #2 stanweld Materials May 9, 2003 2,906 0 0 US You must go to other Codes; e.g. B31.4, B31.8 or regulatory laws such as 49CFR Part 192, etc. Upvote 0 Downvote