Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations The Obturator on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

MMPDS - Aluminum

Status
Not open for further replies.

DrewK

Automotive
Oct 11, 2006
2
Can someone who has access to MMPDS-03 tell me if it has information on 3xxx aluminum? (specifically, 3003).

Thanks.

Drew
 
Replies continue below

Recommended for you

I don't have -03, but since -01 didn't contain anything on 3xxx series, I can't imagine that this has changed. 3xxx series alloys like 3003 are not used for modern aerospace applications. What type of information do you need? There are a lot of other references like ASM HANDBOOK Volume 2, etc. that will have information on mechanical properties, fabrication, etc.
 
Looking for fatigue data, but I think I've found another source...

Thanks!
 
Fatigue Data Book: Light Structural Alloys from ASM has some data on 3003 and 3004.
 