thread507-415433
shore-to-E_z1a1d7.png


Please see the attached image to see a mathcad version of the Ruess formula, taken from a Dow white paper.
 
Replies continue below

Recommended for you

You can develop these for each specific polymer.
But even if you change the compounding too much they no longer apply.
And some polymers just don't follow these relationships.
It is much easier to actually test a sample and get a real number.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 