Hi,
we're designing a 4 cavity thin-wall cup, but we face the problem of mold base deflection. the middle of mold plate(male side) will sink by injection pressure and cause uneven wall-thickness. When mold base sink, mold cores will move toward the center.
we have to put few thin copper sheet (maybe 0.1~0.15mm) in the middle of male side plate to adjust the plate deflection. Is there any better to avoid plate deflection.
Thanks
we're designing a 4 cavity thin-wall cup, but we face the problem of mold base deflection. the middle of mold plate(male side) will sink by injection pressure and cause uneven wall-thickness. When mold base sink, mold cores will move toward the center.
we have to put few thin copper sheet (maybe 0.1~0.15mm) in the middle of male side plate to adjust the plate deflection. Is there any better to avoid plate deflection.