Can someone please tell me what MTLTV stands for? For example: SA516-70N MTLTV. Thanks
 
Replies continue below

Recommended for you

I don't see a SA516-70N MTLTV, I see no listing for 70N only the following. A normal listing is SA516-70MT+LTV.
I see it mostly in Eastern European Listings

ASTM A516-70MT LTV Normalized Condition ASTM A516M-70 MT LTV

ASTM A516 Grade 60/Grade 70 MT+LTV Normalized+Impact Tested+Vacuum Degassed
 