HIC testing is not required for base material with clad or weld overlay. However base material still needs NACE compliance.

Please explain.
 
Replies continue below

Recommended for you

Not required by whom? Oh yes, don't tell me. It's down to the specifier's perception of speed of the degradation mechanisms and the exposed surface area needed to bring them about.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 