NACE MR 0175 deos not address whether HIC is required or not for a material . How to find whether HIC testing is required or not?
 
Replies continue below

Recommended for you

Thank you steve for your reply. I was curious how would I do, if I was end user.
 
You would most likely base the need for HIC testing on the likelihood of this damage mechanism occurring given the product form and chemical composition along with the criticality of the item