Jun 17, 2002 #1 reichertc Mechanical Mar 21, 2001 115 0 0 CA I'm looking for information regarding NDT of plastic pipe welds. I think there was an ASTM standard that covered radiographic and ultrasonic testing of plastic buttwelds (F600??) but it was withdrawn in the 70's. Any current resources available?
I'm looking for information regarding NDT of plastic pipe welds. I think there was an ASTM standard that covered radiographic and ultrasonic testing of plastic buttwelds (F600??) but it was withdrawn in the 70's. Any current resources available?
Jul 12, 2002 #2 Ron Structural Sep 24, 1999 16,336 0 36 US Check with the American Welding Society (http://www.aws.org). They have standards for evaluation of thermoplastic welds. Upvote 0 Downvote
Check with the American Welding Society (http://www.aws.org). They have standards for evaluation of thermoplastic welds.