Hi, I'm looking for a NDT training course. Does anyone know of any good ones that are available? It's mainly ultrasonic testing I'm interested in but would consider a general NDT course. I look forward to hearing from you guys.
 
Replies continue below

Recommended for you

I have always used a company called The South West School of NDT in Cardiff, South Wales. In fact I have just completed and passed PCN Radiography Level 2 and 3 (Aerospace) training and RPS.

I know they also do Composites training.

You will also find a growing list of NDT Training Schools at
I hope this is some help. I hope it goes well with you.
 