Are there chemical composition specs. for this steel? I am hearing that they list only physical specs. for this steel.

 
Replies continue below

Recommended for you

There are limited restrictions placed on HSLA steels according to SAE J2340, but that does not mean composition is completely free. The carbon content is limited to 0.13% max, P & S also have maxima specified, and there is a minimum content of Nb, Ti, or V. You can obtain SAE J2340 either directly from SAE or from a licensed distributor like Global Engineering Documents.
 