cjmann10185
Mechanical
- Aug 26, 2014
- 1
Hello-
I am looking to see if anyone is able to share any information regarding their test methods for in mold label adhesion on injection molded parts. We use a standard cross hatch peel test for pad print, heat transfer, etc but the IML is a different animal since it is a [in this specific application] multi layer PET label.
Thanks in advance.
Chris
I am looking to see if anyone is able to share any information regarding their test methods for in mold label adhesion on injection molded parts. We use a standard cross hatch peel test for pad print, heat transfer, etc but the IML is a different animal since it is a [in this specific application] multi layer PET label.
Thanks in advance.
Chris