Dear All,
i need to know what is the allowable tolerance limits for specimen dimensions for concrete cubes sampled at project site.
as i dont have a copy of above code and the Contractor is claiming that 10% tolerance is allowed as per above code.
can any body confirm or advise if that is o.k.
our test specimen showed sizes of L-156mmxW-150mmxH-150mm with 150 nominal size of concrete cubes and moulds.
any leads to previous threads will be appreciated.
regards,
i need to know what is the allowable tolerance limits for specimen dimensions for concrete cubes sampled at project site.
as i dont have a copy of above code and the Contractor is claiming that 10% tolerance is allowed as per above code.
can any body confirm or advise if that is o.k.
our test specimen showed sizes of L-156mmxW-150mmxH-150mm with 150 nominal size of concrete cubes and moulds.
any leads to previous threads will be appreciated.
regards,