Oct 18, 2009 #1 steve101 Structural Sep 27, 2003 16 0 0 GB can anyone recommend one? I'll check with a few vendors later, but, as usual, if possible, info now is great.
can anyone recommend one? I'll check with a few vendors later, but, as usual, if possible, info now is great.
Oct 18, 2009 1 #2 SJones Petroleum Apr 22, 2001 3,890 1 36 GB http://www.lord.com/Home/ProductsSe...rtoSubstrateAdhesives/tabid/3261/Default.aspx This is the most often specified manufacturer for riser coating primers and related chemicals. Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04 Upvote 0 Downvote
http://www.lord.com/Home/ProductsSe...rtoSubstrateAdhesives/tabid/3261/Default.aspx This is the most often specified manufacturer for riser coating primers and related chemicals. Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04
Nov 10, 2009 #3 LittleNose Mechanical Dec 12, 2003 9 0 0 GB "Rubber and Plastics Industries" in Aberdeen also provide rubber to metal bonding http://www.rpiscotland.co.uk/rubber_metal.html Upvote 0 Downvote
"Rubber and Plastics Industries" in Aberdeen also provide rubber to metal bonding http://www.rpiscotland.co.uk/rubber_metal.html
Nov 10, 2009 #4 Ussuri Civil/Environmental May 7, 2004 1,575 0 0 GB http://www.sba.co.uk/adhes.asp Dunlop S2000 Upvote 0 Downvote