Do we face problems as stated below in non-metallic coating for above ground pipe ?
Non-metallic coating suchas FBE coating is not preferred for above ground pipelines/piping as the change in temperature may lead to dis-attachment from the metal surface.
Lining suchas HDPE may fail due to heating of air in the airgap between internal Dia of metallic and external dia of HDPE