Hello everyone,
I have a stress system in which PSV piping is supported through vessel platform. Please see attached snap. In this stress system, loads at nozzle neck are showing only in Y & z direction forces (FY & FZ), moments (MX). Other force FX and moments MY & MZ are showing as ZERO. Can anybody help me with this? Why is it happening? Is there anything wrong? I checked my input, all the node C-node connections are properly defined.
Piping details: A358 316L CL.1, 10" sch.10S, Ope Temp: 71 deg. F, Max. Design temp.: 150 deg.F, Min. Design Temp.: -20 deg.F
Vessel details: A240 304L, Ope Temp: 71 deg. F, Max. Design temp.: 150 deg.F, Min. Design Temp.: -20 deg.F
Nozzle loads at nozzle neck showing as below:
Node Load Case FX lb. FY lb. FZ lb. MX ft.lb. MY ft.lb. MZ ft.lb.
10350 TYPE=Rigid ANC;
6(SUS) -0 -978 -37 -31.4 0.0 0.0
7(OPE) -0 -939 18 199.0 0.0 0.0
9(OPE) -0 -2520 -1377 -4171.6 0.0 0.0
10(OPE) 0 1104 1108 1812.7 -0.0 -0.0
11(OPE) -0 -938 32 266.9 0.0 0.0
13(OPE) -0 -938 28 249.9 0.0 0.0
15(OPE) -0 -2348 -799 -1563.8 0.0 0.0
16(OPE) 0 1470 -135 -4295.6 -0.0 -0.0
17(OPE) 0 -939 15 187.8 -0.0 -0.0
18(OPE) -0 -939 3 129.6 -0.0 0.0
MAX 0/L10 -2520/L9 -1377/L9 -4295.6/L16 -0.0/L10 -0.0/L10
Thanks
Akash
I have a stress system in which PSV piping is supported through vessel platform. Please see attached snap. In this stress system, loads at nozzle neck are showing only in Y & z direction forces (FY & FZ), moments (MX). Other force FX and moments MY & MZ are showing as ZERO. Can anybody help me with this? Why is it happening? Is there anything wrong? I checked my input, all the node C-node connections are properly defined.
Piping details: A358 316L CL.1, 10" sch.10S, Ope Temp: 71 deg. F, Max. Design temp.: 150 deg.F, Min. Design Temp.: -20 deg.F
Vessel details: A240 304L, Ope Temp: 71 deg. F, Max. Design temp.: 150 deg.F, Min. Design Temp.: -20 deg.F
Nozzle loads at nozzle neck showing as below:
Node Load Case FX lb. FY lb. FZ lb. MX ft.lb. MY ft.lb. MZ ft.lb.
10350 TYPE=Rigid ANC;
6(SUS) -0 -978 -37 -31.4 0.0 0.0
7(OPE) -0 -939 18 199.0 0.0 0.0
9(OPE) -0 -2520 -1377 -4171.6 0.0 0.0
10(OPE) 0 1104 1108 1812.7 -0.0 -0.0
11(OPE) -0 -938 32 266.9 0.0 0.0
13(OPE) -0 -938 28 249.9 0.0 0.0
15(OPE) -0 -2348 -799 -1563.8 0.0 0.0
16(OPE) 0 1470 -135 -4295.6 -0.0 -0.0
17(OPE) 0 -939 15 187.8 -0.0 -0.0
18(OPE) -0 -939 3 129.6 -0.0 0.0
MAX 0/L10 -2520/L9 -1377/L9 -4295.6/L16 -0.0/L10 -0.0/L10
Thanks