can a 3.2 7018 electrode be used on a P 45 alloy pipe
 
Replies continue below

Recommended for you

Yes, for P45 carbon steel helical series pipe.
 
Is this a P No. 45 like Alloy 800, 825, 20, etc? If so then NO.
 