I am trying to establish pressure temperature chart for P92 / F92 material. This material has been in use for more than a decate but not listed under ASME Section II Part D, ASME B31.1 or ASME B31.3.

Please let me know if there is any publication for P92/F92 material which lists the yield, allowable and tensile properties for each temperature range as listed in ASME Section II Part D so that I can determine the pressure and temperature rating of the pressure containing equipment.

 
msmedesign;
Grade P92/F92 is material allowed under an ASME B&PV Code Case, 2179-6. Get yourself a copy of this code case, it has all of the required allowable stress values and restrictions.
 