Hello,

If this forum is not the most adequate to this question, please someone inform me which one is so i can question there.

I was hired to design a steel structure to support a roof and a runway girder. This structure will be located in a sewage treatment station but will not be in constant direct contact with sewage. The runway girder will be used to lift the grill with the wastes one time per day so maybe it will have contact daily with contaminants, although is not immersed.

ETE_tovkns.jpg


At first i thought of specify stainless steel but i'm want to know if there are some solution which is adequate and more economical.

CBCA, which is a steel institute in my country(Brazil) has a guide to painting and surface treatment of steel and this guide has a suggestion of a painting stustem for "steel structures which are immersed in effluent and sewage" that is suitable for carbon steel and weathering steel. This system consists of three layers (150µm each) of coal tar epoxy. My first idea is to specify weathering steel with this painting system.

My question is if a system design for steel immersed in sewage is also adequate and economical for steel that has sporadic contact with sewage.

Thanks in advance.
 
Replies continue below

Recommended for you

The hydrogen sulfide(H2S), methane(CH4) and carbon dioxide(CO2), among others, is vented to the atmosphere... adding to greenhouse gases.

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
My preference for this application would be a high performance paint system, surface prep is important. Enforce the recommendations of the product data sheet for best service life.

My observations are that high performance coatings last as well as heavy hot dip galvanizing except where mechanical abuse damages the coating.

The coating system above is similar to what I would choose. Your market should have similar offerings from local suppliers of industrial coating systems.
 