We have been making some repairs on a sevage treatment tank on a vessel. The tank is built of stainlesss steel and the repairs done with tig welding and stainless steel.
The tank contain apart from sanitary waste also sea water.
It is being painted with International Paint 704. 300 Micron thickness.
The problem is the surface preparation before painting.
Being a stainless steel tank, do we need to dry sand blast, or can we wet blast with high pressure water and sand.
Then dry the tank and paint.
Thank you.
Torben