Hi Guys,
I have an issue with an H2SO4 manual isolation valve (block) upstream of an automated valve. The Automated valve controls H2So4 supply to the H2So4 scrubber vessel.
Trouble is that this manual valve is not operated regularly and during the maintenance of the automated valve, it does not shut off completely and leaking gaseous H2So4 and Cl2 fumes.
The valve data is:
BALL, VALVE; 8" NB (200MM) JAMESBURY FULL BORE: C/W LOCKING DEVICE: ASME CL150RF, A216 WCB CARBON STEEL BODY & CAP; MONEL BALL.
The seat is PTFE or PFA. See the catalogue attached.
The manual valve does not have any other isolation valve upstream. Hence, to change that out, we have to take the train out.
So far, only option, I have is to replace or refurb the valve proactively but that is in a way difficult as there is always a very tight schedule for labour resources during the shut.
So, I am searching for options to find better material, particularly for seating.
Thanks for the help in advance.
Cheers,
Tj
I have an issue with an H2SO4 manual isolation valve (block) upstream of an automated valve. The Automated valve controls H2So4 supply to the H2So4 scrubber vessel.
Trouble is that this manual valve is not operated regularly and during the maintenance of the automated valve, it does not shut off completely and leaking gaseous H2So4 and Cl2 fumes.
The valve data is:
BALL, VALVE; 8" NB (200MM) JAMESBURY FULL BORE: C/W LOCKING DEVICE: ASME CL150RF, A216 WCB CARBON STEEL BODY & CAP; MONEL BALL.
The seat is PTFE or PFA. See the catalogue attached.
The manual valve does not have any other isolation valve upstream. Hence, to change that out, we have to take the train out.
So far, only option, I have is to replace or refurb the valve proactively but that is in a way difficult as there is always a very tight schedule for labour resources during the shut.
So, I am searching for options to find better material, particularly for seating.
Thanks for the help in advance.
Cheers,
Tj