PAUT VS RT COST

Status
Not open for further replies.

fgonza5750

Industrial
Oct 13, 2012
1
Our subcontractors want use phase array in liue RT, we are wondering the impact cost at the project, and the benefits in early finish at the project.

In my opinion we just get improve in safety,

we are not working at night shift, so the impact for man power is not a concern.


Some body here have a study or idea in reference at it?
 
Replies continue below

Recommended for you

Phase array is faster and doesn't require exclusion zone. IMO better than RT when wall thickness is high.
Disadvantages - no physical record, dependent on operator, can be problematic on stainless.
 
If this is an unplanned and unscheduled change, then be aware of the following:

1. The end user may require qualification of the subcontractor. If they demand a 'full blown' qualification, then the premise that an early finish is a possibility will go out of the window.


and for pipelines, try this one:


2. Setting acceptance criteria

Steve Jones
Materials & Corrosion Engineer


All answers are personal opinions only and are in no way connected with any employer.
 