Chemical
Nov 9, 2017
2
I have an order that has been delayed by 2 months from the manufacturer. The order is for SST ball valves with PCTFE (Kel-F) seats and 6" pups. The order is shipping from Italy so I am looking at another 4 week delay. Is there anything that can be done to a standard SST ball valve as modification for the seat and pups at a local machine shop?
 