Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PEEK Piston Cap Instead of PTFE?

Status
Not open for further replies.

MechyMarco

Mechanical
Jun 5, 2014
39
Wondering if anyone has used PEEK for a piston seal on here? Application is for a linear seal. Normal design is a standard slipper seal with o-ring underneath a ring of PTFE to energize. If I replace the PTFE with PEEK it should still work I think. Benefit is increased extrusion resistance and wear resistance. Been using carbon graphite PTFE and it's failing due to wear mainly.
 