My question is that in high temperature service, how does carbon affect the phyical properties of stainless steel metallurgically?
A personal observation. I have seen a lot more failures in high pressure feedwater heaters made with 304N than with 304 or 304L. I feel that it is due to the higher allowed stress of the 304N (which is in reality 304LN) resulting in a lower effective saftey factor. I can't prove this, but I believe it.