Hello,
During annealing of rolled metal rings at around 840 c , I have a problem that some rings show intens physical deformation! I could use some tips of how to go about this!
thanks
During annealing of rolled metal rings at around 840 c , I have a problem that some rings show intens physical deformation! I could use some tips of how to go about this!