Clamont
Mechanical
- Dec 10, 2012
- 40
I am trying to read through ASME IX to qualify some welders and have some queries on the ranges qualified;
1. QW-452.3 - This states that the smaller diameter pipes automatically qualify the larger pipes... For example if the welder is qualified on a 1" pipe they are also qualified for 20"? It seems not to make sense to me however I cannot find anything else with conditions to this.
2. Does a pipe groove weld automatically qualify for a plate groove weld... If so where is this stated?
Thanks
1. QW-452.3 - This states that the smaller diameter pipes automatically qualify the larger pipes... For example if the welder is qualified on a 1" pipe they are also qualified for 20"? It seems not to make sense to me however I cannot find anything else with conditions to this.
2. Does a pipe groove weld automatically qualify for a plate groove weld... If so where is this stated?
Thanks