Hi what pipe materials i need to use for boiler piping, in places having low ambient temp?
For example boiler when operating, will have temp, above 500 deg C
But when it is shut down, the piping comes down to ambient conditions say -10 deg C
What ASME Section I or any other codes says about this?
Will th material be prone to brittle fracture then?
What conditions shall be considered and how safety shall be incorporated?