Which are the best electrodes to weld these grades of steel pipes ????

Pipe welding of S355j2(+ N) with api 5L x60 ?
 
Replies continue below

Recommended for you

For the SMAW process, E7016/E7018 can be used. If full penetration from one side is required, E7010 should be used at least for the root and second pass.

 