Pitting corrosion on material ASME / ASTM A-240 A1

Status
Not open for further replies.

Alcinei

Industrial
Oct 24, 2002
3
Does anybody know if the material ASME / ASTM A-210 A1 is susceptible to pitting corrosion when submitted to salty environment?

Thanks in advance!

Alcinei Nery
 
Replies continue below

Recommended for you

ASME SA 210 A1 is carbon steel tubing. I am not sure what you mean by a "salty" environment. If you are referring to sea water or a marine coast type of environment, the carbon steel will develop corrosion pits on the surface exposed to the environment.
 