I am trying to get up to speed ASAP on the state of the art for bulk weld cladding of large steel components for corrosion and/or wear resistance by PTAW + powder alloy. I am not talking about valve seats and the like, I am interested in cladding by the acre on plate and large-diameter pipe. Info on welding equipment makers, consumable vendors and welding parameters are welcomed, including published papers/texts.