Does ASME B31.3 Appendix X preclude testing a bellows expansion joint pneumatically at a reduced pressure as is permitted throughout the rest of the code for other components?






 
Replies continue below

Recommended for you

The pressure test in Appendix X is designed to prove the expansion joint pressure design. You can test it pneumatically, but the pressure is not reduced. Same pressure is required, either hydrostatic test or pneumatic test.
 