24
We'd like to test the hardness of a generator shaft after a shrink fit assembly. The generator is about 200kg and is difficult to test on a regular Rockwell tester. I'm considering renting a portable hardness tester but have no experience with them. Are they reliable? How accurate they are? Any specific types or brands you can recommend? Thanks.
 
Replies continue below

Recommended for you

On machined surfaces the portable hardness testers work well. To check reproducibility and accuracy standard blocks are available along with the tester.

This service is largely provided by the NDT agencies in India,overseas too it might be the same.

Equotip is one such brand .

 
What is your accuracy requirement?

I use a portable kit from :
It is part number 1342T13 and currently sells for just under 700 bucks. Its advertised accuracy is +/- 1.5 HRC

It's accuracy is highly dependant on your eyesight, but I would say I can determine within 2 points fairly easily.

I have found it to come up with readings very close to my regular machine.
 
I have been using Equotip portable hardness tester for last 9 years and strongly recommend it.



Rao Yallapragada
 
We have found the telebrinell hardness testers to be the most reliable and cost affective portable hardness testers for field work.
 
We have had problems in the past with Equotip and Telebrinell testers. These have risen mainly from people trying to use them when the work piece is not big enough or well supported.

We have also experienced people using the machine on an alloy which does not have a hardness conversion scale available, and so getting some very wrong hardness values and rejecting material as a result of this.

You should be OK if you follow the instructions, and are working with carbon and low-alloy steels.
 
Gentlemen, I've rented a Krautkramer Dynapocket and it worked fine for the parts that we tested. Thanks for all your replies and suggestions.
 